965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance

BLOOM(suzhou) Materials Co.,Ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now
    Buy cheap 965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance from wholesalers
     
    Buy cheap 965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance from wholesalers
    • Buy cheap 965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance from wholesalers

    965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance

    Ask Lasest Price
    Brand Name : BLM-DX-1
    Price : FobShanghai usd 5.9-6.4/kg
    Payment Terms : Western Union, L/C, T/T
    Supply Ability : 300 Ton/Tons per Month
    Delivery Time : 25-30 days subject to the clients' requirement and quantity
    • Product Details
    • Company Profile

    965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance

    Inconel 718

    Inconel 718 Chemical composition


    Alloy%NiCrFeMoNbCoCMnSiSCuAlTi
    718Min.5017balance2.84.750.20.7
    Max.55213.35.510.080.350.350.010.30.81.15

    Inconel 718 Physical properties


    Density8.2 g/cm³
    Melting point1260-1340 ℃

    Inconel 718 Alloy minimum mechanical properties in the roomtemperature


    AlloyTensile strength Rm N/mm²Yield strength R P0. 2N/mm²Elongation A 5 %

    Brinell hardness

    HB

    Solution treatment96555030≤363

    718 Characteristic as below:

    1.workability

    2.High tensile strength,endurance strength,creep strength and rupture strength at 700℃.

    3.High inoxidability at1000℃. 4.Steady mechanical performance in the low temperature.

    5.Good welding performance.


    Inconel 718 Metallurgical structure


    718alloy is Austenitic structure, precipitation hardening generate "γ" made it excellent mechanical performance. G rain boundary generate "δ" made it the best plasticity in the heat treatment.


    Inconel 718 Corrosion resistance


    718 alloy with extremely resistance to stress corrosion cracking and pitting ability in high temperature or low temperature environments, especially the inoxidability in the high temperature.


    Inconel 718 Application field:

    1 . The elevated temperature strength, excellent corrosion resistance and workability at 700℃ properties

    2 . made it use in a wide range of high requirement environments :Steam turbine ; Liquid-fuel rocket ; Cryogenic engineering

    3.Acid environment

    4.Nuclear engineering



    Quality 965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: BLOOM(suzhou) Materials Co.,Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)